The Influence of Impurities on the Properties of Lead Part V - Creep Tests on Electrolytic Lead and some of its Alloys

This paper contains an account of some creep tests on electrolytic lead and some of its alloys. The stresses used in determining creep were 500, 350, and 200 lb. per sq.' in. The alloys contained silver, bismuth, tellurium, antimony and zinc respectively. All were castin vacuo, and tested "as rolled." Tests were done also on electrolytic lead which had been cast in air.The electrolytic lead contained 0.0005% total impurities.The preparation and vacuum casting of this lead have been described in a previous paper in this series. The preparation of the alloys, and the air casting of the electrolytic lead, are described in the next section.EXPERIMENTAL PROCEDURE.Every effort was made to keep the vacuum-cast specimens from contact with the atmosphere throughout their history.The ingots were stored eIther in a vacuum desiccator or immersed in heavy oil. The creep specimens were coated with vaseline except during rolling, etching and photography, which involved exposure to the atmosphere for about 45 minutes all told.It is not claimed that vaseline is a perfect shield against the intrusion of atmospheric gases. Possibly during the months that some tests were in progress the gases diffused through the vaseline and gained a limited access to the lead.Nevertheless, the use of vaseline gave protection that brought the tests nearer the ideal at which the author aimed, *Research Fellow, Dept. of Metallurgy, University of Melbourne.
Return to parent product
  • The Influence of Impurities on the Properties of Lead Part V - Creep Tests on Electrolytic Lead and some of its Alloys
    PDF
    This product is exclusive to Digital library subscription
  • The Influence of Impurities on the Properties of Lead Part V - Creep Tests on Electrolytic Lead and some of its Alloys
    PDF
    Normal price $22.00
    Member price from $0.00
    Add to cart

    Fees above are GST inclusive

PD Hours
Approved activity
  • Published: 1935
  • PDF Size: 0.789 Mb.
  • Unique ID: P_PROC1936_0421

Our site uses cookies

We use these to improve your browser experience. By continuing to use the website you agree to the use of cookies.