Skip to main content
Conference Proceedings

The AusIMM Proceedings 1988

Conference Proceedings

The AusIMM Proceedings 1988

PDF Add to cart

Technical Note-Deposit Morphology and Current Efficiency in Electrolytic Zinc Deposition

The presence of impurities which are electropositive to zinc in acid zinc electrolyte causes changes to deposit morphology and reduced current efficiency. Glue may be added to control some impurity effects, but assaying for animal glue concentration is difficult and seldom done. Measurement of the activation overpotential for zinc deposition by cyclic voltammetry is used in some plants to monitor electrolyte quality and control glue additions.The deposit morphology and current efficiency of zinc deposition from commercial electrolyte were investigated for various glue additions in the presence of increased levels of antimony. Cyclic voltammetry was investigated as a method of optimising glue additions in the presence of antimony.Scanning electron rnicroscopy showed deposits characteristic of the impurity element present and the glue addition rate. Cyclic voltarnmetry measurements showed some correlation between current efficiency and activation polarisation potential. The importance of using tankhouse electrolytes where results are to be related to tankhouse operation was noted.
Return to parent product
  • Technical Note-Deposit Morphology and Current Efficiency in Electrolytic Zinc Deposition
    PDF
    This product is exclusive to Digital library subscription
  • Technical Note-Deposit Morphology and Current Efficiency in Electrolytic Zinc Deposition
    PDF
    Normal price $22.00
    Member price from $0.00
    Add to cart

    Fees above are GST inclusive

PD Hours
Approved activity
  • Published: 1988
  • PDF Size: 0.435 Mb.
  • Unique ID: P_PROC1988_1728

Our site uses cookies

We use these to improve your browser experience. By continuing to use the website you agree to the use of cookies.