Development of the All-Flotation Process at the Zinc Corporation Limited, Broken Hill (Reprint)

The ore mined from the Lead Lode of The Zinc Corporation leases consists of a fairly granular mixture of galena, marmatite, chalcopyrite, tetrahedrite, pyrrhotite, pyrite, and lollingite with a gangue association of calcite, quartz, bustamite, rhodonite, mangan-hedenbergite, garnet, fluorite, mangano-calcite and apatite. The silver content of the ore occurs in three minerals tetrahedrite, dyscrasite, and pyrargyrite, the last two mentioned occurring in microscopic association only. Other metallic and gangue minerals are also present in this complex mineralogical association, but do not influence the milling operations.Fortunately, the silver minerals favour the galena and chalcopyrite as their host minerals, thus facilitating the recovery of both copper and silver in the lead concentrate. The ore from the Lead Lode assays from 14 - 18 per cent lead; 3.0 - 4.5 oz silver per tonne, and 9.5 - 12.0 per cent zinc.A parallel lode, known as the Zinc Lode, is well developed in The Zinc Corporation leases. This lode assays from six to eight per cent lead, 1.5 oz silver per ton, 18 - 25 per cent zinc with a siliceous gangue. The common Lead Lode gangue minerals, calcite, rhodonite, bustamite - are very rare in present underground exposures. No metallurgical work was done on this ore during the pilot plant operations.The aim in the milling process is to produce:1. A lead concentrate with the maximum economic recovery of lead, silver, gold, copper and antimony, and minimum zinc content.2. A zinc concentrate with the maximum economic recovery of zinc, cadmium, and cobalt, and minimum iron, arsenic and fluorine content.3. A waste residue containing sufftcient granular material to be utilised as underground fill.In considering the economics of the milling practice the above three requirements plus consideration of the tariffs submitted by the purchasers of concentrates were the deciding factors in the evolution of the present milling practice.Towards the end of 1924 The Zinc Corporation Limited added to and adapted the old zinc tailings plant for the treatment of 5000 tons of crude ore per week. This plant, which operated until January 1936, was in general principles similar to the standard Broken Hill methods of ore concentration, whereby the galena was recovered by the gravity concentration methods of jigging and tabling with selective flotation concentration of the residual galena and marmatite. One important difference from other Broken Hill plants was that the primary grinding of the jig tailing was performed with flint-loaded mills operating in closed circuit with revolving screens. Two primary grinding sections were installed, each consisting of two 5 ft diameter by 10ft long tube mills loaded with flint pebbles working in closed circuit with four 3 ft diameter by 3 ft wide revolving screens covered with 22mesh Toncap woven wire screen with 0.57 mm opening. Each section carried a circulating load of 28.3 tons per hour for a jig.
Return to parent product
  • Development of the All-Flotation Process at the Zinc Corporation Limited, Broken Hill (Reprint)
    PDF
    This product is exclusive to Digital library subscription
  • Development of the All-Flotation Process at the Zinc Corporation Limited, Broken Hill (Reprint)
    PDF
    Normal price $22.00
    Member price from $0.00
    Add to cart

    Fees above are GST inclusive

PD Hours
Approved activity
  • Published: 1994
  • PDF Size: 0.69 Mb.
  • Unique ID: P_PROC1994_1811

Our site uses cookies

We use these to improve your browser experience. By continuing to use the website you agree to the use of cookies.